Stainless Steels Manual Electrode E312-17 ore isikebhe weld
UBUCHWEPHESHE bokushisela
Ungavumeli imibuzo
Qhubeka nokukuhlupha
Ukungazinzi kwe-arc
Ukubumba okungabukeki
I-spatter eyeqile
Ifanele zonke izinhlobo zensimbi eqinile kanye nokuqina
i-alloy steel okunzima ukuyishisela futhi kulula ukuqhekeka noma ibe ne-porosity
Uhlobo lwe-Acid olunezigaba ezimbili zensimbi engenasici yesandla, i-jet arc,
ingxenye eyinhloko ingu-29%Cr-9%Ni, evame ukwaziwa ngokuthi "i-electrode yendawo yonke.
Ripple kahle
Ukusebenza kahle kwe-welding, i-arc ezinzile, ukwakheka okuhle,
i-ripple ethambile, i-splash encane, ukususwa kwe-slag kalula.
I-coating inokumelana okuhle nomlilo, ukumelana okuhle kwe-porosity, kanye nezakhiwo ezinzile zemishini yensimbi ehlanganisiwe
I-slagging elula
Ipharamitha Yomkhiqizo
COMPONET YECHEMICAL:
I-ALLOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Cu | Okunye |
GB/T IMITHETHO | 0.057 | 1.1 | 0.74 | 0.026 | 0.005 | 9.8 | 28.4 | 0.07 | 0.11 | - |
IMPAHLA YOMKHETHI:
IMPAHLA | UKUVUMELA AMANDLA(MPa) | AMANDLA AMANDLA(MPa) | IMAPACT VALUE J/℃ | Ukwelashwa kokushisa °C*h | ||||
GB/T IMITHETHO | 800 | 25 | - | - |
IMIPHAKATHI YOKUSHISA ENCONYWAYO:
IZINCACISO ZAMA-DIAMETERS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
Ugesi (Amp) | H/W | 30-55 | 50-85 | 80-120 | 100-150 | 140-180 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
Ukwesekwa kwefekthri
Umkhiqizo ufanele a
anhlobonhlobo izicelo
UBUCHWEPHESHE bokushisela
-
2.3 million imiphongolo
I-SBM Fast4ward FPSO
-
I-GDS-2209/GXS-E330
indawo yokubeka i-tube
Hainan Huasheng
phenol recovery tower
COMPONET YECHEMICAL:
I-ALLOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Cu | Okunye |
GB/T IMITHETHO | 0.057 | 1.1 | 0.74 | 0.026 | 0.005 | 9.8 | 28.4 | 0.07 | 0.11 | - |
IMPAHLA YOMKHETHI:
IMPAHLA | UKUVUMELA AMANDLA(MPa) | AMANDLA AMANDLA(MPa) | IMAPACT VALUE J/℃ | Ukwelashwa kokushisa °C*h | ||||
GB/T IMITHETHO | 800 | 25 | - | - |
IMIPHAKATHI YOKUSHISA ENCONYWAYO:
IZINCACISO ZAMA-DIAMETERS(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
Ugesi (Amp) | H/W | 30-55 | 50-85 | 80-120 | 100-150 | 140-180 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |